welding current : 40-280A
model number : E6013
application : Carbon Steel
Type : AWS A5.1 E6013
Tensile Strength : ≥430Mpa
Elongation : ≥16%
Current: AC+/DC
Carbon Steel Welding Electrode
The welding of duplex stainless steel is primarily utilized in the offshore oil and gas,
natural gas, and petrochemical industries.
Notes:
1. The appropriate current range is suitable for both AC and DC welding.
2. Dry the electrodes at 100°C to 150°C for 30 to 60 minutes.
3. Clean the contaminants on the base material to reduce welding defects.
4. Apply an appropriate current to prevent deterioration of X-ray and mechanical properties.
| Chemical Composition | C | Mn | Si | S | P | V | Ni | Cr | Mo |
| Guarantee Value | ≤0.20 | ≤1.2 | ≤1.00 | ≤0.035 | ≤0.04 | ≤0.08 | ≤0.3 | ≤0.20 | ≤0.3 |





Contact: admin
Phone: +86-13665233012
E-mail: service@weldmaterial.com